Hi guys! I’m a new member, looking for advice on how I can complete my metal finishing project effectively and safely.
I had some custom post-beam ties for an outdoor deck made from 1/4" 304 stainless at SendCutSend (laser cut, press-brake bent, and deburred). Imagine an upper-case “T”, with the sides of the top-bar of the “T” angled back 12 or 30 degrees. Now I need to put a #4 finish (i.e. a brushed stainless steel finish) on the front surface. I’ve got a linear sander (an Eastwood Contour SCT) with the appropriate abrasive drums, and I’ve watched YouTube videos of folks getting that kind of finish with that kind of tool.
My first uncertainty is how and where to clamp down my workpieces so I can finish their fronts without a lot of clamping and unclamping. We have fixturing tables in the welding areas, but the pieces won’t lie flat because of the bends. I could potentially make wood cradles or something to hold them more securely, but maybe I’m missing some easier solution? It would be especially nice if I could clamp the pieces upright or at an angle, to make them easier to work on.
My second uncertainty is whether such a finishing job would generate too much dust to do in the shop at all. I noticed the woodshop has a downdraft table, but there doesn’t seem to be anything like that in the metal shop. Maybe I should be doing this whole thing outside?
There is a yellow exhaust fan over each welding area which you can re-position. The lever has to be open for the air to flow. For clamping, you could find some random things in the scrap bins, like angle iron, and use that along with the fixture clamps. You can google “fixture table accessories” for workholding ideas. Don’t sand the fixture table! Metal dust is heavier than wood dust and falls to the floor. Just sweep up it afterwards. I wouldn’t worry about it being too much. If you want to make a mess, you need steel objects that’s been stored outside and covered with rust. You have no rust and therefore will not be converting metal shop into Mad Max.
If the plates are 1/4” thick, you can likely hold them in one of the vices, for example: 3/16” of the material engaged in the jaws, with 1/16” proud of the vice for surfacing. Graining takes very little pressure so you don’t need it to be bombproof.
I like that idea. I should come in and go through the available vises to see what might work. I might need to take some care against cross-contamination – maybe we have some vise jaw inserts that would prevent iron-to-stainless contact.